I. Corrosion

1           The effect of magnesium on the corrosion behavior of sputter-deposited amorphous Al-Mg-Ti ternary alloys in a neutral chloride solution

E. Akiyama, H. Yoshioka, J. H. Kim, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 34, 27-44 (1993).

2           Preparation of protective alumina coating on austenitic stainless steel by sol-gel method

Y. Wang, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Zairyo-to-Kankyo [Corros. Eng.], 42 [3], 158-165 (1993).  (in Japanese)

ゾル・ゲル方により316ステンレス鋼上に作製したアルミナ被覆の保護性

王穎,秋山英二,幅崎浩樹,川嶋朝日,浅見勝彦,橋本功二

材料と環境,42 [3], 158-165 (1993).

3           The corrosion behavior of sputter-deposited amorphous titanium-chromium alloys in 1 M and 6 M HCl solutions

J. H. Kim, E. Akiyama, H. Yoshioka, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 34, 975-988 (1993).

4           Corrosion-resistant chromium-valve metal alloys

K. Hashimoto, J. H. Kim, E. Akiyama, H. Habazaki, A. Kawashima and K. Asami

Proc. 12th International Corrosion Congress, Vol. 3A, 1102-1110 (1993).

5           Effect of rinsing on analytical results for passivity of amorphous iron-chromium-metalloid alloys

K. Hashimoto, S. Kato, B.-M. Im, E. Akiyama, H. Habazaki, A. Kawashima and K. Asami

                     Proc. 12th International Corrosion Congress, Vol. 5B, 3940-3950 (1993).

6           The corrosion behavior of sputter-deposited amorphous chromium-zirconium alloys in 6 M HCl solution

J. H. Kim, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 34, 1817-1827 (1993).

7           Electrochemical and XPS studies of effects of alloying elements on the corrosion behavior of amorphous Fe-Cr-metalloid alloys in 9 M H2SO4

B.-M. Im, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 34, 1829-1839 (1993).

8           The corrosion behavior of sputter-deposited amorphous Cr-Nb and Cr-Ta alloys in 12 M HCl solution

J. H. Kim, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 34, 1947-1955 (1993).

9           The corrosion behavior of sputter-deposited amorphous Al-Ti-Ni alloys in 1 M HCl solution

E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion, Electrochemistry and Catalysis of Metastable Metals and Intermetallics, (ed. C. R. Clayton and K. Hashimoto), p.26-37, The Electrochemical Society, Pennington, NJ (1993).

10         The corrosion behavior of sputter-deposited amorphous Al-Cr alloys

J. H. Kim, E. Akiyama, H. Yoshioka, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion, Electrochemistry and Catalysis of Metastable Metals and Intermetallics, (ed. C. R. Clayton and K. Hashimoto), p.48-59, The Electrochemical Society, Pennington, NJ (1993).

11         An XPS study of the corrosion behavior of sputter-deposited amorphous Cr-Nb and Cr-Ta alloys in 12 M HCl solution

J. H. Kim, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 36, 511-523 (1994).

12         Highly corrosion-resistant amorphous Cr-Ni-P alloys

B.-P. Zhang, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng. A181/A182, 1114-1118 (1994).

13         Effect of phosphorus on the passivation behavior of amorphous Fe-8Cr-13P-7C alloy in 9 M H2SO4 solution

B.-M. Im, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng. A181/A182, 1119-1122 (1994).

14         The corrosion behavior of sputter-deposited amorphous Ni-Ti alloys in 1 M HCl solution

E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng. A181/A182, 1128-1132 (1994).

15         The corrosion behavior of sputter-deposited amorphous Cr-Ni-Mo alloys in 12 M HCl solution

P. Y. Park, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 36, 1395-1410 (1994).

16         The corrosion behavior of amorphous Fe-8Cr-13P-7C and Fe-8Cr-20P alloys in concentrated sulfuric acid

B. M. Im, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 36, 1537-1550 (1994).

17         Preparation of protective multilayer SiO2 and Al2O3 coatings on austenitic stainless steel by sol-gel method

A. Kawashima, Y. Wang, E. Akiyama, H. Habazaki, K. Asamim and K. Hashimoto

Zairyo-to-Kankyo [Corros. Eng.], 43[11], 654-659 (1994).

18         The corrosion behavior of sputter-deposited amorphous Mo-Zr alloys in 12 M HCl

P. Y. Park, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 37, 307-320 (1995).

19         The effect of phosphorus addition on the corrosion behavior of amorphous Ni-30Ta-P alloys in 12 M HCl

H. J. Lee, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 37, 321-330 (1995).

20         Change in the surface composition of amorphous Fe-Cr-Mo-P-C alloys during air exposure

M.-W. Tan, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 37, 331-341 (1995).

21         The effect of phosphorus addition on the corrosion behavior of amorphous Fe-8Cr-P alloys in 9 M H2SO4

B.-M. Im, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 37, 709-722 (1995).

22         Similarity and difference in roles of chromium and molybdenum in passivating amorphous alloys in concentrated acids

K. Hashimoto, P. Y. Park, J. H. Kim, E. Akiyama, H. Habazaki, A. Kawashima and K. Asami

Mater. Sci. Forum, 185-188, 779-788 (1995).

23         Indoor atmospheric corrosion behavior of rapidly quenched amorphous Zr-Cu alloys

K. Asami, E. Akiyama, Y. Murakami, H. M. Kimura, M. Kikuchi and K. Hashimoto

Mater. Sci. Forum, 185-188, 789-798 (1995).

24         The corrosion behavior of sputter-deposited amorphous Al-Cr-Ti alloys in 1 M HCl 

E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Forum, 185-188, 809-818 (1995).

25         The effect of air exposure on the corrosion behavior of amorphous Fe-8Cr-Mo-13P-7C alloys in 1 M HCl

M.-W. Tan, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto             

Corrosion Science, 37, 1289-1302 (1995).

26         The effect of phosphorus on the passivation behavior of Ni-10Ta-P alloys in 12 M HCl

H. J. Lee, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 37, 1313-1324 (1995).

27         The effect of microcrystallites in the amorphous matrix on the corrosion behavior of amorphous Fe-8Cr-P alloys

B. M. Im, M. Komori, B.-T. Lee, E. Aoyagi, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami, K. Hiraga and K. Hashimoto

Corrosion Science, 37, 1411-1422 (1995).

28         The corrosion behavior of sputter-deposited Cr-Mo alloys in 12 M HCl solution

P. Y. Park, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 37, 1843-1860 (1995).

29         The corrosion behavior of sputter-deposited amorphous W-Ti alloys in 6 M HCl solution

J. Bhattarai, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 37, 2071-2086 (1995).

30         The corrosion behavior of sputter-deposited amorphous Al-Cr-Mo alloys in 1 M HCl

E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 279-292 (1996).

31         The Influences of Mo addition and air exposure on the corrosion behavior of amorphous Fe-8Cr-13P-7C alloy in deaerated 1 M HCl

M.-W. Tan, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 349-365 (1996).

32         High temperature sulfidation and oxidation behavior of sputter-deposited Al-refractory metal alloys

H. Mitsui, E. Akiyama, A. Kawashima, K. Asami, K. Hashimoto and S. Mrowec

Materials Transaction, JIM, 37, 379-382 (1996).

33         The corrosion behavior of Ni-Ta-5P alloys in concentrated hydrochloric acid

H.-J. Lee, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Materials Transaction, JIM, 37, 383-388 (1996).

34         The effect of phosphorus addition on the corrosion behavior of arc-melted Ni-10Ta-P alloys in 12 M HCl

H.-J. Lee, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 469-485 (1996).

35         The corrosion behavior of sputter-deposited Mo-Ta alloys in 12 M HCl solution

P. Y. Park, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 397-411 (1996).

36         A study of the structure of a passive film using angle-resolved X-ray photo-electron spectroscopy

E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 1127-1140 (1996).

37         The corrosion behavior of amorpous and crystalline Ni-10Ta-20P alloys in 12 M HCl

H. J. Lee, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 1269-1279 (1996).

38         The effects of alloying elements on passivity of sputter-deposited amorphous Al-Cr-Mo alloys in 1 M HCl

E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 1281-1294 (1996).

39         The influences of pre-immersion on the polarization behavior of amorphous Fe-Cr-Mo-P-C Alloy in deaerated 1 M HCl

M.-W. Tan, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 1495-1511 (1996).

40         The corrosion behavior of sputter-deposited Mo-Ti alloys in concentrated hydrochloric acid

P. Y. Park, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 1649-1667 (1996).

41         The corrosion behavior of sputter-deposited Mo-Nb alloys in 12 M HCl solution

P. Y. Park, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 1731-1750 (1996).

42         The role of chromium and molybdenum in passivation of amorphous Fe-Cr-Mo-P-C alloys in deaerated 1 M HCl

M.-W. Tan, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 38, 2137-2151 (1996).

43         XPS study of Ni-Mo-B amorphous Ultra-fine particles prepared by chemical reduction

J. Saida, E. Akiyama, K. Hashimoto, A. Inoue and T. Masumoto

J. Japan Inst. Metals, 60, 79-83 (1996).  (in Japanese)

             化学還元法で作製したNI-Mo-B非晶質合金超微粒子のX線光電子分光法による解析

才田淳次,秋山英二,橋本功二,井上明久,増本健

日本金属学会誌, 60 [1], 79-83 (1996).

44         The corrosion behaviour of sputter-deposited amorphous Mn-Ti alloys in 0.5 M NaCl solutions

A. A. El-Moneim, B.-P. Zhang, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 39, 305-320 (1997).

45         The roles of tantalum and phosphorus on the corrosion behaviorof Ni-Ta-P alloys in 12 M HCl"

H.-J. Lee, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 39, 321-332 (1997).

46         Electrochemical and XPS studies of the corrosion behavior of sputter-deposited amorphous W-Zr alloys in 6 and 12 M HCl solutions

J. Bhattarai, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami And K. Hashimoto

Corrosion Science, 39, 355-375 (1997).

47         The effect of molybdenum on the stability of passive films formed on amorphous Fe-Cr-Mo-P-C alloys by potentiostatic polarization in deaerated M HCl"

M.-W. Tan, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 39, 589-603 (1997).

48         Spontaneously passivated films on sputter-deposited Cr-Ti alloys in 6 M HCl solution

X.-Y. Li, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 39, 935-948 (1997).

49         An angle-resolved XPS study of the in-depth structure of passivated amorphous aluminum alloys

E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 39, 1351-1364 (1997).

50         An XPS study of passive films on corrosion-resistant Cr-Zr alloys prepared by sputter deposition

     X.-Y. Li, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

     Corrosion Science, 39, 1365-1380 (1997).

51         The sulphidation and oxidation behavior of sputter-deposited Cr-refractory metal alloys at high temperatures

H. Habazaki, K. Ito, H. Mitsui, E. Akiyama, A. Kawashima, K. Asami, K. Hashimoto and S. Mrowec

Mater. Sci. Eng., A226-228, 910-914 (1997).

52         Corrosion-resistant amorphous aluminum alloys and structure of passive films

E. Akiyama, H. Habazaki, A. Kawashima, K. Asami, K. Hashimoto

Mater. Sci. Eng., A226-228, 920-924 (1997).

53         The corrosion behavior of sputter-deposited amorphous Mn-Ta alloys in 0.5 M NaCl solutions

A. A. El-Moneim, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and  K. Hashimoto

Corrosion Science, 39, 1965-1979 (1997).

54         The corrosion behavior of Ni-Cr-Mo ternary alloys in hot concentrtated sulfuric acids with active carbon (Part 1)

K. Sugawara, Y. Takizawa, E. Akiyama and K. Hashimoto

Zairyo-to-Kankyo [Corros. Eng.], 46, 643-650 (1997).  (in Japanese)

             活性炭を含む高温・濃硫酸中におけるNi-Cr-Mo合金の腐食挙動(第1報)

菅原活生,滝沢与司夫,秋山英二,橋本功二

材料と環境, 46, 643-650 (1997).

55         The corrosion behavior of Ni-Cr-Mo ternary alloys in hot concentrtated sulfuric acids with active carbon (Part 2)

K. Sugawara, Y. Takizawa, E. Akiyama and K. Hashimoto

Zairyo-to-Kankyo [Corros. Eng.], 46, 702-708 (1997).  (in Japanese)

             活性炭を含む高温・濃硫酸中におけるNi-Cr-Mo合金の腐食挙動(第2報)

菅原活生,滝沢与司夫,秋山英二,橋本功二

材料と環境, 46, 702-708 (1997).

56         Electrochemical and XPS studies on the passivation behavior of sputter-deposited W-Cr alloys in 12 M HCl solution

J. Bhattarai, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 40, 155-175 (1998).

57         Electrochemical and XPS studies on the corrosion behavior of sputter-deposited W-Nb alloys in concentrated hydrochloric acid solutions

J. Bhattarai, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 40, 19-42 (1998).

58         An experimental evidence of the critical size of heterogeneity for pitting corrosion of Cr-Zr alloys in 6 M HCl

M. Mehmood, B.-P. Zhang, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 40, 1-17 (1998).

59         Passivity and its breakdown of sputter-deposited amorphous Mn-Zr alloys in neutral chloride solutions

A. A. El-Moneim, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and  K. Hashimoto

Corrosion Science, 40, 235-250 (1998).

60         XPS study of transformation of air-formed film to passive film on sputter deposited Mo-Nb alloys in 12 M HCl

D. Huerta, P.-Y. Park, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Proc. Symposium on Passivity and Its Breakdown, p.770-780, The Electrochemical Society, Pennington, NJ (1998).

61         The passivation behavior of sputter-deposited W-Ta alloys in 12 M HCl

J. Bhattarai, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 40, 757-779 (1998).

62         An XPS study of passive films on sputter-deposited Cr-Nb alloys in 12 M HCl solution

X.-Y. Li, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 40, 821-838 (1998).

63         The effect of alloying elements on the corrosion behavior of sputter-deposited amorphous Mn-Ta-Cr alloys in 1 N H2SO4

A. A. El-Moneim, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 40, 1491-1512 (1998).

64         XPS and electrochemical studies on the corrosion behaviour of sputter-deposited amorphous Mn-Nb alloys in a neutral chloride solution

A. A. El-Moneim, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and  K. Hashimoto

Corrosion Science, 40, 1513-1532 (1998).

65         Electrochemical and XPS studies of the passivation behavior of sputter-deposited amorphous Cr-Ta alloys in 12 M HCl

X.-Y. Li, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and  K. Hashimoto

Corrosion Science, 40, 1587-1604 (1998).

66         The influence of concentration of hydrochloric acid solutions on the passivation behavior of sputter-deposited tungsten rich W-Nb alloys

J. Bhattarai, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 40, 1897-1914 (1998).

67         Change in pitting susceptibility with alloy heterogeneity induced by crystallization of amorphous alloys

M. Mehmood, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Forum, 289-292, 629-640 (1998).

68         The critical size and nature of nanocrystalline heterogeneity for pitting corrosion 

K. Hashimoto, M. Mehmood, X.-Y. Li, E. Akiyama, H. Habazaki, A. Kawashima and K. Asami

Proc. Symp. Critical Factors in Localized Corrosion III, p.245-255, The Electrochemical Society, Pennington, NJ (1998).

69         The effect of heat treatment on the corrosion behavior of sputter-deposited aluminum-chromium alloys

M. Mehmood, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 41, 477-499 (1999).

70         Electrochemical and XPS studies of the corrosion behavior of sputter-deposited amorphous Fe-Cr-Ni-Nb alloys in 6 M HCl

X.-Y. Li, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and  K. Hashimoto

Corrosion Science, 41, 1095-1118 (1999).

71         The corrosion behavior of sputter-deposited amorphous Fe-Cr-Ni-Ta alloys in 12 M HCl

X.-Y. Li, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 41, 1849-1869 (1999).

72         The degradation of the corrosion resistance of sputter-deposited chromium-titanium alloys by nanoscale heterogeneity

M. Mehamood, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 41, 1871-1890 (1999).

73         The sulfidation and oxidation behavior of sputter-deposited Al-Mo-Nb alloys

K. Hon-yashiki, H. Habazaki, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng., A267, 277-284 (1999).

74         Corrosion-resistant Mn-Zr-Cr alloys in chloride-containing media

A. A. El-Moneim, E. Akiyama, H. Habazaki, A. Kawashima, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng., A267, 285-293 (1999).

75         The influence of dichromate ions on aluminum dissolution kinetics in artificial crevice electrode cells

E. Akiyama and G. S. Frankel

J. Electrochem. Soc., 146, 1095 (1999).

76         Effects of nanocrystalline heterogeneity on the corrosion behavior of sputter-deposited chromium-niobium alloys

M. Mehmood, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Corrosion Science, 42, 361-382 (2000).

77         Release of chromate ions from chromate conversion coatings on Al alloys

E. Akiyama, L. Xia, R. McCreery, A. Markworth and G. S. Frankel

Proc. on "Passivity and Localized Corrosion", (M. Seo, B. MacDougall, H. Takahashi and R. G. Kelly Eds.) The Electrochemical Society pp300-309 (2000).

78         Oxidation Behavior of Amorphous Ni-Zr and Ni-Zr-Rare Earth Element Alloys

M. Yamasaki, H. Habazaki, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Per Kofstad Memorial Symposium on High Temperature Corrosion and Materials Chemistry (P.Y. Hou, T. Maruyama, M.J. McNallan, T. Narita, E.J. Opila and D.A. Shores Eds.) The Electrochemical Society pp180-191 (2000).

79         Angle-resolved XPS for determination of diffusion coefficients and mobilities of cations in thin passive films

K. Asami, E. Akiyama and K. Hashimoto

Surf. Int. Anal., 30, 106-111 (2000).

80         XPS determination of diffusion coefficients of cations in thin passive films on alloys

K. Asami, E. Akiyama and K. Hashimoto

Solid State Phenomena, 72, 79-84 (2000).

81              Strage and release of soluble hexavalent chromium from chromate conversion coatings

Equilibrium aspects of CrVI concentration

Lin Xia, Eiji Akiyama, Gerald Frankel and Richard McCreery

J. Electrochem. Soc., 147, 2556-2562 (2000).

82         Enhancement of corrosion resistance of amorphous aluminum alloys by alloying additions

Eiji Akiyama, Katsuhiko Asami, Hiroki Habazaki, Asahi Kawashima and Koji Hashimoto

Proc. on “Corrosion and Corrosion Protection”, J. D. Sinclair, E. Kalman, M. W. Kendig, W. Plieth, W. H. Smyrl, Eds., The Electrochemical Society, Pennington, NJ, p1-8 (2001).

83         塑性域の軸力で締付けて海浜暴露したボルト内の吸蔵水素分布

阪下真司,秋山英二,津崎兼彰,松山晋作

鉄と鋼88, 35-42 (2002).

             Distribution of hydrogen occluded in bolts tightened beyond the yield strength and exposed at a seashore site

Shinji Sakashita, Eiji Akiyama, Kaneaki Tsuzaki and Shinsaku Matsuyama

Tetsu-to-Hagané, 88, 35-42 (2002).

84         Storage and release of soluble hexavalent chromium from chromate conversion coatings on Al alloys; Kinetics of release

E. Akiyama, A. J. Markworth, J. K. McCoy, G. S. Frankel, L. Xia and R. L. McCreery

J. Electrochem. Soc., 150, B83-B91 (2003).

85         A study of current transients caused by single particle impact on electrodes

E. Akiyama, A. W. Hassel, M. Stratmann

Proc. on Asian-Pacific Corrosion Control Conference, Asian-Pacific Materials & Corrosion Association, 027 (2003).

86         Electrochemical transients caused by single particle impacts

Eiji Akiyama, Achim W. Hassel, Martin Stratmann

Proc. on “Second International Conference on Advanced Structural Steel”, CMS, CISRI & BAO STEEL, Shanghai, China, pp.911-914 (2004).

87         Estimation of delayed fracture resistance of high strength steels

Maoqiu Wang, Eiji Akiyama, Keitaro Enami, Kaneaki Tsuzaki

Proc. on “Second International Conference on Advanced Structural Steel”, CMS, CISRI & BAO STEEL, Shanghai, China, pp.646-649 (2004).

88         Hydrogen absorption behavior of high strength steels under atmospheric corrosion

Katsuhiro Matsukado, Eiji Akiyama, Kaneaki Tsuzaki

Proc. on “Second International Conference on Advanced Structural Steel”, CMS, CISRI & BAO STEEL, Shanghai, China, pp.323-326 (2004).

89         Hydrogen degradation of a boron-bearing steel with 1050 and 1300 MPa strength levels

Maoqiu Wang, Eiji Akiyama, Kaneaki Tsuzaki

Scripta Materialia, 52, 403-408 (2005).

90         Crosshead speed dependence of the notch tensile strength of a high strength steel in the presence of hydrogen

Maoqiu Wang, Eiji Akiyama, Kaneaki Tsuzaki

Scripta Materialia, 53, 713-718 (2005).

91         Effect of hydrogen and stress concentration on the notch tensile strength of AISI 4135 steel

Maoqiu Wang, Eiji Akiyama, Kaneaki Tsuzaki

Materials Science and Engng A, 398, 37-46 (2005).

92         Repassivation of titanium under particle impingements

E. Akiyama and K. Tsuzaki

Proc. on “16th International Corrosion Congress”, on CD P-18-B-2 (2005).

92         Evaluation of hydrogen embrittlement of high strength by slow strain rate test

Maoqiu Wang, Eiji Akiyama, Kaneaki Tsuzaki

Proc. on “16th International Corrosion Congress”, on CD P-10-H-14 (2005).

93         Hydrogen distribution inside the crevice and the variation with applied potential

Thiyagarajan Sundararajan, Eiji Akiyama, Kaneaki Tsuzaki

Proc. on “16th International Corrosion Congress”, on CD P-10-H-16 (2005).

94         Hydrogen mapping across crevice: Effect of applied potential

Thiyagarajan Sundararajan, Eiji Akiyama, Kaneaki Tsuzaki

Scripta Materialia, 53, 1219-1223 (2005).

95         Hydrogen mapping across crevice

Thiyagarajan Sundararajan, Eiji Akiyama, Kaneaki Tsuzaki

ELECTROCHEMICAL AND SOLID STATE LETTERS, 8, No. 9, B30-B33 (2005).

96         Effect of hydrogen on the fracture behavior of high-strength Cr-Mo steel

Maoqiu Wang, Eiji Akiyama, Kaneaki Tsuzaki

Materials Science Forum, 512, 55-60 (2006).

97         Acetate and chloride Effects on hydrogen production across the crevice

Thiyagarajan Sundararajan, Eiji Akiyama, Kaneaki Tsuzaki

Materials Science Forum, 512, 97-102 (2006).

98         A fracture criterion for hydrogen embrittlement of a high strength steel

Maoqiu Wang, Eiji Akiyama, Kaneaki Tsuzaki

Materials Science and Technology, 22, 2, 167-172 (2006).

99         Determination of the critical hydrogen concentration for delayed fracture of high strength steel by constant load test and numerical calculation

Maoqiu Wang, Eiji Akiyama, Kaneaki Tsuzaki

Corrosion Science, 48, 2189-2202 (2006).

100       Depassivation and repassivation of titanium under particle impingements

E. Akiyama and K. Tsuzaki

ECS Transitions, 1, 4, 437-446 (2006).

101       Discrete electrochemical transients of aluminium alloys generated by slurry jet impingement

E. Akiyama, A. W. Hassel, M. Stratmann

Jouurnal of Physics D: Applied Physics, 39, 3157-3164 (2006).

102       Hydrogen entry in crevice region: Evaluation by hydrogen permeation technique

T. Sundararajan, E. Akiyama and K. Tsuzaki

ISIJ International, 46, 7, 1081-1085 (2006).

103       Hydrogen embrittlement problems in high strength steel bolts

Thiyagarajan Sundararajan, Eiji Akiyama, Kaneaki Tsuzaki

Proc. on “International Corrosion Congress, CORCON 2005”, NACE international India Section, Chennai, India (2005), ts-15-1 on CD.

104       Evaluation of Delayed Fracture Properties of High Strength Steels for Bolts

E. Akiyama, M.Q. Wang, K. Matsukado, Z.G. Zhang, T. Sundararajan and K. Tsuzaki

Proc. on “The 3rd International Conference on Advanced Structural Steels, Gyeongju, Korea, August 22-24, 2006

105       Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test

Maoqiu Wang, Eiji Akiyama, Kaneaki Tsuzaki

Corrosion Science, submitted.

106       Corrosion behavior of Al-7wt% Si-1.5wt% Cu severely deformed by equal-channel angular pressing

Zuogui Zhang, Eiji Akiyama, Yoshimi Watanabe, Yasuyuki Katada and Kaneaki Tsuzaki

Materials Science Forum, accepted.

107       Influence of microstructure on electrochemical properties of severely deformed Al-5 wt% Cu alloy by ECAP

Zuogui Zhang, Eiji Akiyama, Yoshimi Watanabe, Yasuyuki Katada and Kaneaki Tsuzaki

Materials Science Forum, accepted.

108       Effect of a-Al/Al3Ni microstructure on the corrosion behaviour of Al-5.4 wt% Ni alloy fabricated by equal-channel angular pressing

Zuogui Zhang, Eiji Akiyama, Yoshimi Watanabe, Yasuyuki Katada and Kaneaki Tsuzaki

Corrosion Science, submitted.

 

 

 

II. Electrodes

1           Amorphous alloy electrodes for anodic oxidation of sulfite

T. Mori, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng. A181/A182, 1081-1084 (1994).

2           Amorphous alloy electrodes for electro-oxidation of propane

H. Kishimoto, A. Kawashima, E. Akiyama, K. Asami and K. Hashimoto

Sci. Rep. Res. inst. Tohoku University, A41, 83-88 (1995).

3           Effect of cathodic reaction on catalytic activity of amorphous alloy electrodes for electrooxidation of sulfite

T. Mori, A. Kawashima, E. Akiyama, H, Habazaki, K. Asami and K. Hashimoto

J. Appl. Electrochem. 25, 953-961 (1995).

4           Characterization of sputtre-deposited Ni-Mo and Ni-W alloy electochatalysts for hydrogen evolution in alkaline solution

A. Kawashima, E. Akiyama, H. Habazaki and K. Hashimoto

Mater. Sci. Eng. A226-228, 905-909 (1997).

5           Surface activation of manganese oxide electrode for oxygen evolution in electrolysis of seawater

K. Izumiya, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

J. Appl. Electrtochem. 27, 1362-1368 (1997).

6           Effects of additional elements on the electrocatalytic properties of thermally decomposed manganese oxide electrodes for oxygen evolution from seawater

K. Izumiya, E. Akiyama, H. Habazaki, N. Kumagai, A. Kawashima and K. Hashimoto

Mater. Trans. JIM, 38, 899-905 (1997).

7           Mn-W oxide anodes prepared by thermal decomposition for oxygen evolution in seawater electrolysis

K. Izumiya, E. Akiyama, H. Habazaki, N. Kumagai, A. Kawashima and K. Hashimoto

Mater. Trans. JIM, 39, 308-313 (1997).

8           Anodically deposited manganese oxide and manganese-tungsten oxide electrodes for oxygen evolution from seawater

K. Izumiya, E. Akiyama, H. Habazaki, N. Kumagai, A. Kawashima and K. Hashimoto

Electrochimica Acta, 43, 3303-3321 (1998).

9           Hydrogen evolution characteristics of sputter-deposited Co-Mo, Co-Al and Co-Mo-Al alloy electrodes in NaOH solution

T. Aihara, A. Kawashima, E. Akiyama, H. Habazaki, K. Asami and K. Hashimoto

Mater. Trans. JIM 39, 1017-1023 (1998).

10         Oxygen evolution anodes in seawater electrolysis for global CO2 recycling

K. Izumiya, K. Fujimura, E. Akiyama, H. Habazaki, A. Kawashima and K. Hashimoto

Proc. on EUROMAT'98, Conf. on Materials in Oceanic Environment, The Federation of European Materials Sciences, (1998) pp.37-45.

11         Anodically deposited manganese-molybdenum oxide anodes with high selectivity for evolving oxygen in electrolysis of seawater

K. Fujimura, K. Izumiya, A. Kawashima, H. Habazaki, E. Akiyama, N. Kumagai and K. Hashimoto

J. Appl. Electrochem. 29 765-771 (1999).

12         Oxygen evolution anodes in seawater electrolysis

K. Fujimura, T. Matsui, K. Izumiya, N. Kumagai, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng. A267, 254-259 (1999).

 

 

III. Catalysts

1           Decomposition of nitrogen monoxide over amorphous Co-65Zr alloys containing platinum group elements

M. Komori, H. Habazaki, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Materials Transaction, JIM, 34, 725-731 (1993).

2           Nitrogen monoxide decomposition catalysts prepared from amorphous Co-Zr-Pd alloys

M. Komori, H. Habazaki, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion, Electrochemistry and Catalysis of Metastable Metals and Intermetallics, (ed. C. R. Clayton and K. Hashimoto), p.369-380, The Electrochemical Society, Pennington, NJ (1993).

3           Amorphous alloys for hydrolysis of CCl2F2

A. Hirota, K. Ebidzuka, H. Habazaki, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Corrosion, Electrochemistry and Catalysis of Metastable Metals and Intermetallics, (ed. C. R. Clayton and K. Hashimoto), p.381-392, The Electrochemical Society, Pennington, NJ (1993).

4           Decomposition of CCl2F2 through hydrolysis by amorphous alloy catalysts

K. Ebidzuka, H. Habazaki, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng. A181/A182, 1091-1094 (1994).

5           Nitrogen monoxide decomposition catalysts prepared from amorphous Ni-valve metal-Pd alloys

M. Komori, H. Habazaki, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng. A181/A182, 1123-1127 (1994).

6           Amorphous Fe-valve metal-platinum group metal alloy catalysts for methanation of carbon dioxide

T. Tada, H. Habazaki, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng. A181/A182, 1133-1136 (1994).

7           Decomposition of nitrogen monoxide over palladium-supported NiTa2O6 catalysts prepared from amorphous alloy precursors

M. Komori, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Appl. Catal. B, Environmental, 9, 93-106 (1996).

8           The microcomposite structure of catalysts prepared by oxidation of amorphous Ni-Ta-Pd alloys

B.-P. Zhang, K. Funayama, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Materials Transactions, JIM, 38, 123-132 (1997).

9           NO decomposition catalysts prepared from amorphous No-Ta-Pd alloys

M. Komori, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Appl. Catal. B, Environmental, 11, 243-255 (1997).

10         CO2 methanation catalysts prepared from amorphous Ni-Zr alloy precursors

K. Shimamura, M. Komori, H. Habazaki, T. Yoshida, M. Yamasaki, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Supple. to Mater. Sci. Eng., A226-228, 376-379 (1997).

11         Application of sputter deposition technique to the preparation of amorphous alloy-derived catalysts for NO decomposition

K. Funayama, H. Habazaki, E. Akiyama, A. Kawashima, K. Asami, K. Hashimoto and M. Komori

Mater. Trans. JIM, 38, 643-649 (1997).

12         Composition dependence of the CO2 methanation activity of Ni/ZrO2 catalysts prepared from amorphous Ni-Zr alloy precursors

M. Yamasaki, H. Habazaki, T. Yoshida, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Appl. Catal. A, General 163, 187-197 (1997).

13         Methanation of carbon dioxide on catalysts derived from amorphous Ni-Zr-rare earth element alloys

H. Habazaki, T. Yoshida, M. Yamasaki, M. Komori, K. Shimamura, E. Akiyama, A. Kawashima and K. Hashimoto

Studies in Surf. Sci. Catal. 114, 261-266 (1998).

14         Characterization of CO2 methanation catalysts prepared from amorphous Ni-Zr and Ni-Zr-rare earth element alloys

M. Yamasaki, H. Habazaki, T. Yoshida, M. Komori, K. Shimamura, E. Akiyama, A. Kawashima, K. Asami and K. Hashimoto

Studies in Surf. Sci. Catal. 114, 451-454 (1998).

15         CO2 methanation catalysts prepared from amorphous Ni-Zi-Sm and Ni-Zr-mish metal alloy precusors

 M. Yamasaki, M. Komori, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Hashimoto

Mater. Sci. Eng. A267, 220-226 (1999).

16         Materials for global carbon dioxide recycling

K. Hashimoto, M. Yamasaki, S. Meguro, T. Sasaki, H. Katagiri, K. Izumiya, N. Kumagai, H. Habazaki, E. Akiyama and K. Asami

Corrosion Science,,, 44, 371-386 (2002).

 

 

IV. Reviews

1           Corrosion-resistant amorphous surface alloys

K. Hashimoto, N. Kumagai, H. Yoshioka, J. H. Kim, E. Akiyama, H. Habazaki, S. Mrowec, A. Kawashima and K. Asami

Corrosion Science, 35, 363-370 (1993).

2           Recent progress in corrosion-resistant metastable alloys

K. Hashimoto, P. Y. Park, J. H. Kim, H. Yoshioka, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami, Z. Grzesik and S. Mrowec

Mater. Sci. Eng. A198, 1-10 (1995).

3           Recent progress in corrosion-resistant new alloys prepared by sputter deposition

K. Hashimoto, H. Habazaki, E. Akiyama, H. Yoshioka, J. H. Kim, P. Y. Park, A. Kawashima, and K. Asami

Sci. Rep. Res. inst. Tohoku University, A42, 99-105 (1996).

4           Substantiation plant of global CO2 recycling

K. Hashimoto, H. Habazaki and E. Akiyama

J. Soc. Mat. Sci., Japan, 45, 1067-1068 (1996).  (in Japanese)

CO2リサイクル実証プラント

橋本功二,幅崎浩樹,秋山英二

材料, 45 [9], 1067-1068 (1996).

5           Global CO2 recycling

K. Hashimoto, E. Akiyama, H. Habazaki, A. Kawashima, K. Shimamura, M. Komori and N. Kumagai

Zairyo-to-Kankyo [Corros. Eng.], 45 [10], 614-620 (1996).  (in Japanese)

             グローバルCO2リサイクル

橋本功二,秋山英二,幅崎浩樹,川嶋朝日,嶋村和郎,古森充,熊谷直和

材料と環境, 45 [10], 614-620 (1996).

6           Roles of chromium, molybdenum and tungsten in spontaneous passivity of sputter-deposited single phase alloys in concentrated hydrochloric acids

K. Hashimoto, J.-H. Kim, P.-Y. Park, J. Bhattarai, E. Akiyama, H. Habazaki, A. Kawashima and K. Asami

Proc. 13th Int. Cong. Corrosion, paper 444, 1-10 (1996).

7           The role of phosphorus in enhancing corrosion resistance of amorphous alloys

K. Hashimoto, B. P. Zhang, B.-M. Im, H. J. Lee, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami

Sci. Rep. Res. inst. Tohoku University, A43 (1997) 145-151.

8           Global CO2 recycling

K. Hashimoto, E. Akiyama, H. Habazaki, A. Kawashima

ECO INDUSTRY, 2 [2], 5-14 (1997).  (in Japanese)

グローバルCO2リサイクル

     橋本功二,秋山英二,幅崎浩樹,川嶋朝日

     月刊エコインダストリー, 2 [2], 5-14 (1997).

9           Energy balance of global CO2 recycling and amounts of reduction of CO2 emission

K. Hashimoto, E. Akiyama, H. Habazaki, A. Kawashima, M. Komori, K. Shimamura and N. Kumagai

Sci. Rep. Res. inst. Tohoku University, A43[2], 153-160 (1997).

10         Global CO2 recycling

K. Hashimoto, K. Izumiya, E. Akiyama, H. Habazaki, A. Kawahima, K. Shimamura, M. Komori, N. Kumagi

CERAMIC DATA BOOK '97, 25, 108-116 (1997).  (in Japanese)

             グローバル二酸化炭素リサイクル

橋本功二,泉屋宏一,秋山英二,幅崎浩樹,川嶋朝日,嶋村和郎,古森充,熊谷直和

CERAMIC DATA BOOK '97, 25, 108-116 (1997).  (in Japanese)

11         Electrochemistry and Corrosion Engineering of Global CO2 Recycling

K. Hashimoto, K. Izumiya, K. Fujimura, M. Yamasaki, E. Akiyama, H. Habazaki, A. Kawashima, M. Komori, K. Shimamura and N. Kumagai

Proc. CORROSION 98 Research Topical Symposium on Corrosion in Advanced Materials and Systems, NACE, pp.1-14 (1998).

12         Sputter-deposited amorphous and nanocrystalline alloys with extremely high corrosion resistance

K. Hashimoto, H. Mitsui, J. Bhattarai, P.-Y. Park, J.-H. Kim, X.-Y. Li, A. A. El-Moneim, E. Akiyama, H. Habazaki, A. Kawashima and K. Asami

Proc. 4th Special Symposium on Advanced Materials, pp.51-54 (1998)

13         Spontaneously passivated sputter-deposited alloys with higher corrosion resistance than alloy components

K. Hashimoto, J. Bhattarai, X.-Y. Li, P.-Y. Park, J.-H. Kim, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and K. Shimamura

Proc. Symposium on Passivity and Its Breakdown, p.369-383, The Electrochemical Society, Pennington, NJ (1998).

14         Global CO2 Recycling  -Novel Materials, Reduction of CO2 Emission, and Prospect-

K. Hashimoto, K. Izumiya, K. Fujimura, M. Yamasaki, E. Akiyama, H. Habazaki, A. Kawashima, M. Komori, K. Shimamura and N. Kumagai

Advances in Materials, Mater. Sci. Eng. A267, 200-206 (1999).

15         Global CO2 Recycling

K. Hashimoto, M. Yamasaki, K. Fujimura, T. Matsui, K. Izumiya, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami and N. Kumagai

SODA & CHLORINE, 50, 224-232 (1999).  (in Japanese)

             グローバル二酸化炭素リサイクル

橋本功二,山崎倫昭,藤村和也,松井徹郎,泉屋宏一,秋山英二,幅崎浩樹,川嶋朝日,浅見勝彦,熊谷直和

ソーダと塩素 (SODA & CHLORINE), 50 224-232 (1999).

16         Spontaneously passive amorphous Fe-Cr-Ni-Ta alloys in 12 M HCl

K. Hashimoto, X-Y Li, E. Akiyama, H. Habazaki, A. Kawashima and K. Asami

Proc. 14th Int. Cong. Corrosion Paper No.400, p.1-10 (1999).

17         Global CO2 Recycling -To avoid global warming and to supply abundant energy-

K. Hashimoto, M. Yamasaki, T. Matsui, K. Izumiya, S. Meguro, A. Sasaki, H. Katagiri, E. Akiyama, N. Kumagai, H. Habazaki, A. Kawashima. K. Asami

ELECTRO-HEAT, 111, 1-9 (2000).  (in Japanese)

             グローバル二酸化炭素リサイクル −地球温暖化防止と豊富なエネルギー供給のために−

橋本功二,山崎倫昭,松井徹郎,泉屋宏一,目黒眞作,佐々木昭仁,片桐洋,秋山英二,熊谷直和,幅崎浩樹,川嶋朝日,浅見勝彦

エレクトロヒート, 111, 1-9 (2000).

18         Spontaneously passive alloys prepared by sputter deposition using targets consisting of Type 304 stainless steel and valve metals.

K. Hashimoto, X.-Y. Li, K. Shimamura, E. Akiyama, H. Habazaki, A. Kawashima and K. Asami

Proc. 8th Int. Symp. Passivity (2000) in press.

19         Global CO2 Recycling- Novel Materials, Reduction of CO2 Emission, and Prospect-

K. Hashimoto, K. Izumiya, K. Fujimura, M. Yamasaki, E. Akiyama, H. Habazaki, A. Kawashima, M. Komori, K. Shimamura and N. Kumagai

     Advances in Materials, Springer Verlag (2000) in press.

20         Global CO2 recycling using solar energy and hydrolysis of sea water

Koji Hahimoto, Michiaki Yamasaki, Shinsaku Meguro, Teruhito Sasaki, Hiroshi Katagiri, , Eiji Akiyama, Naokazu Kumagai, Hiroki Habazaki, Asahi Kawashima and Katsuhiko Asami

Kaiyou Kaihatsu News, 28, 3-8 (2000).  (in Japanese)

             太陽エネルギーと海水電解を利用するグローバル二酸化炭素リサイクル

橋本功二,山崎倫昭,泉屋宏一,目黒眞作,佐々木昭仁,片桐洋,秋山英二,熊谷直和,幅崎浩樹,川嶋朝日,浅見勝彦

海洋開発ニュース,28, 3-8 (2000).

21         Global carbon dioxide recycling

Koji Hahimoto, Michiaki Yamasaki, Shinsaku Meguro, Teruhito Sasaki, Hiroshi Katagiri, Naokazu Kumagai, Koichi Izumiya, Hiroki Habazaki, Eiji Akiyama, Asahi Kawashima and Katsuhiko Asami

Hyomen Gijutsu, 52, 195-200 (2001).  (in Japanese)

グローバル二酸化炭素リサイクル

橋本功二,山崎倫昭,目黒眞作,佐々木昭仁,片桐洋,熊谷直和,泉屋宏一,幅崎浩樹,秋山英二,川嶋朝日,浅見勝彦

表面技術, 52, 195-200 (2001).

22         Tailoring Electrodes and catalysts for CO2 recycling plant

Koji Hashimoto, Shinsaku Meguro, Teruhito Sasaki, Hiroshi Katagiri, Michiaki Yamasaki, Koichi Izumiya, Naokazu Kumagai, Hiroki Habazaki, Asahi Kawashima , Katsuhiko Asami and Eiji Akiyama

Materia, 40, 372-375 (2001).  (in Japanese)

             CO2リサイクルプラント用電極および触媒の創製

橋本功二,目黒眞作,佐々木昭仁,片桐洋,山崎倫昭,泉屋宏一,熊谷直和,幅崎浩樹,川嶋朝日,浅見勝彦,秋山英二

まてりあ, 40, 372-375 (2001).

23         Advanced materials for global carbon dioxide recycling

Koji Hashimoto, Hiroki Habazaki, Michiaki Yamasaki, Shinsaku Meguro, Teruhito Sasaki, Hiroshi Katagiri, Tetsuro Matsui, Kazuya Fujimura, Koichi Izumiya, Naokazu Kumagai, and Eiji Akiyama

Materials Science and Engineering, A304-306, 88-96 (2001).

 

 

V. Organic Chemistry

1           Total synthesis and absolute configuration of (-)-sedacryptine

E. Akiyama and M. Hirama

                     Synlett, 100-102 (1996).

 

 

VI. Patents

1           Cathode material for hydrogen generation

     K. Hashimoto, K. Hayashi, E. Akiyama, A. Kawashima, K. Asami

     Application numbr : 06085736

     Publication number : 07268676

     Date of publication of application : 17.10.1995

1.          水素発生用陰極材料

橋本功二,林 桂三,秋山英二,川嶋朝日,浅見勝彦

出願日1994331日 特願平6-085736特開平5-

公開番号: 特開平07-268676

公開日: 19951017

2                   Amorphous alloy catalyst for nitrogen decomposition

                     K. Hashimoto, M. Komori, A. Kawashima, K. Asami, H. Habazaki, E. Akiyama

                     Application numbr : 06237087

                     Publication number : 08099039

                     Date of publication of application : 16.04.1996

3                   Oxygen generation electrode

                     K. Hashimoto, K. Izumiya, K. Asami, A. Kaashima, E. Akiyama

                     Application numbr : 07085530

4                   Oxygen generation electrode

                     K. Hashimoto, K. Izumiya, E. Akiyama, A. Kawashima

                     Application numbr : 08064539

5                   Amorphous alloy catalyst for conversion of carbon dioxide into methane

                     K. Hashimoto, M. Komori, K. Shimamura, T. Yoshida, H. Habazaki, E. Akiyama

                     Application numbr : 08204543

                     Publication number : 10043594

                     Date of publication of application : 17.02.1998

6                   Oxygen generation electrode

                     K. Hashimoto, K. Izumiya, E. Akiyama, T. Yoshida, M. Komori, K. Shimamura

                     Application numbr : 08310094

7                   Amorphous alloy catalyst for conversion of carbon dioxide into methane

                     K. Hashimoto, M. Komori, K. Shimamura, T. Yoshida, H. Habazaki, E. Akiyama

                     Application numbr : 09051598

                     Publication number :10244158

                     Date of publication of application : 14.09.1998

8                   Oxygen generation electrode and its production

                     K. Hashimoto, K. Izumiya, E. Akiyama, H. Habazaki, A. Kawashima, K. Asami

                     Application numbr : 09033513

                     Publication number : 10287991

                     Date of publication of application : 27.10.1998

9                   Amorphous alloy catalyst for reformed gas hydrocarbon and use of the catalyst

                     K. Hashimoto, H. Habazaki, E. Akiyama, H. Chiyou, T. Yoshida, T. Yamazaki, K. Ishii, S. Kono

                     Application numbr : 09087241

                     Publication number : 10263400

                     Date of publication of application : 06.10.1998

10                 Method for electrolyzing aqueous solution containing chlorine ion to produce oxygen and hydrogen and electrolytic device

                     K. Hashimoto, K. Izumiya, E. Akiyama, A. Kawashima, N. Kumagai, Y. Samata

                     Application numbr : 10058702

                     Publication number : 11256383

                     Date of publication of application : 21.09.1999

11                 Oxygen generation electrode and its production method

                     K. Hashimoto, K. Izumiya, E. Akiyama, A. Kawashima, N. Kumagai

                     Application numbr : 10058704

                     Publication number : 11256385

                     Date of publication of application : 21.09.1999

 

 

 

 

 

2 NOx分解用アモルファス合金触媒

橋本功二,小森 充,川嶋朝日,浅見勝彦,幅崎浩樹,秋山英二

出願日1994年9月30日 特願平6-237087  特開平8-99039

公開番号: 特開平08-099039

公開日: 1996年04月16日

 

3 酸素発生用電極 

橋本功二,泉屋宏一,浅見勝彦,川嶋朝日,秋山英二

 出願年月日 平成7年11月x日 特願平7-85530

 

4 酸素発生用電極

橋本功二,泉屋宏一,秋山英二,川嶋朝日,浅見勝彦

 出願年月日 平成8年 特願平8-64539

 

5 二酸化炭素のメタン化用アモルファス合金触媒

橋本功二,幅崎浩樹,秋山英二,吉田 健,小森 充,嶋村和郎 

 出願年月日 平成8年8月2日 特願平08-204543号

公開番号: 特開平10-043594

公開日: 1998年02月17日

 

6 酸素発生用電極

橋本功二,泉屋宏一,秋山英二,幅崎浩樹,川嶋朝日,浅見勝彦

 出願年月日 平成8年11月21日 特願平8-310094

 

7 二酸化炭素のメタン化用アモルファス合金触媒

橋本功二,幅崎浩樹,秋山英二,吉田 健,小森 充,嶋村和郎 

 出願年月日 平成9年3月6日 特願平9-51598号

特開平10-244158 平成10年9月14日

公開番号: 特開平10-244158

 

8 酸素発生用電極とその作製方法

橋本功二,泉屋宏一,秋山英二,幅崎浩樹,川嶋朝日,浅見勝彦

 出願年月日 平成9年2月18日 特願平9-33513

公開番号: 特開平10-287991

公開日: 1998年10月27日

 

9 炭化水素改質ガス用アモルファス合金触媒とその用法

橋本功二,幅崎浩樹,秋山英二, 張波萍,吉田健,山崎倫昭,石井宏治,河野駿平

 出願年月日 平成9年3月24日 特願平9-87241

公開番号: 特開平10-263400

公開日: 1998年10月06日

 

10 塩素イオンを含有する水溶液を電解して酸素と水素を発生する電解方法および電解装置 

橋本功二,泉屋宏一 ,秋山英二,川嶋朝日,熊谷直和,佐俣芳光

 出願年月日 平成10年3月10日 特願平10-58702 特開平11-256383

公開番号: 特開平11-256383

公開日: 1999年09月21日

出願番号: 特願平10-058702

 

11 酸素発生用電極とその製造方法

橋本功二,泉屋宏一,秋山英二,川嶋朝日,熊谷直和

 出願年月日 平成10年3月10日 特願平10-58704 特開平11-256385

公開番号: 特開平11-256385

公開日: 1999年09月21日